parallax background image

Five common injection molding defects and how to prevent them

Published On: 10 November 2026 Reading time : 4 minutes

Injection molding is a precise process. Material, design, mold and machine settings all have to match exactly. If one of those links is off, you will see it in the product. A part warps, does not fill completely or breaks sooner than expected.

In this blog, we discuss five defects that often occur in practice, where they come from and how to prevent them.

Why defects often arise before production starts

Many injection molding defects only become visible at the machine, but the cause usually lies earlier. In the design, in the material selection or in the construction of the mold. At the machine, process settings can correct a lot, but not everything.

That makes the difference between fixing and preventing significant. A defect spotted in the design phase costs a change to a drawing. Discovering the same defect once the mold is finished often means a mold modification, extra trial runs and delays.

The five most common defects

Warping

A product that should come out of the mold straight, but is bent or twisted. Warping occurs when parts of the product shrink unevenly. This happens, for example, with large differences in wall thickness, uneven cooling in the mold or an unfavorable gate location. With glass-fiber-reinforced plastics, the orientation of the fibers also plays a role.

You prevent it with a uniform wall thickness, a well-designed cooling system and a material that suits the requirements for dimensional stability. If a product needs to stay very straight, it is best to choose a plastic with low mold shrinkage.

Flow lines and weld lines

When the plastic has to flow around a hole or recess in the mold, two flow fronts meet again on the other side. A weld line forms at that spot. It is often visible as a line on the surface, but more importantly, it is also a mechanically weaker spot.

It cannot always be avoided completely, but you can determine where the weld line ends up. By choosing the gate location carefully, you place it where it is not visible and carries little load. Good venting and the right temperatures also help the flow fronts fuse properly.

Incomplete filling

Sometimes the material does not fill the mold completely. A piece of the edge is missing, a rib is incomplete or a detail is not sharp. This can be caused by walls that are too thin combined with long flow paths, a material that flows less easily, insufficient pressure or air that cannot escape from the mold.

A flow simulation shows in advance whether the product fills properly and where the most difficult points are. It also helps to match the wall thickness to the material, because not every plastic is suitable for very thin-walled products.

Loss of properties due to excessive pressure

If the material is forced through an opening that is too narrow with too much force, a lot of friction builds up in the material. This can damage the long molecules in the plastic. The product may look fine, but is more brittle or weaker than the material promises on paper. Sometimes it can also be recognized by discoloration.

You prevent this with a gate and runners that are large enough for the material and the product, and with process settings that do not put unnecessary strain on the material. Here too, a well-designed mold eliminates many problems at the source.

Insufficiently pre-dried material

A number of plastics absorb moisture from the air, such as PET, PA, PC and PBT. If that material is not dried properly before processing, the moisture in the melt reacts with the plastic. The result is silver streaks, bubbles or a product that is more brittle than it should be.

PET is a good example. Everyone knows it from soft drink bottles, and it is a strong and versatile material. But outside the bottle, it is a challenging material to injection mold. Pre-drying is critical, it flows less easily and the mold needs good cooling. Pre-drying itself is not complicated, but it does need to be well organized, with the right temperature and drying time for the specific material.

Prevention starts in the design phase

Most of these defects have one thing in common. They are easiest to solve before the mold is built. These points help:

  • Align material and design early. Every material has its own limits for wall thickness, shrinkage and flow.
  • Design with a uniform wall thickness. This prevents uneven shrinkage and makes the product easier to fill.
  • Choose the gate location deliberately. It determines how the material flows and where weld lines form.
  • Simulate in advance. A flow simulation reveals warping, filling problems and weld lines before any steel is machined.
  • Make agreements about material preparation. Especially with moisture-sensitive and recycled plastics, pre-drying and inspecting the material is essential.

Working together towards a defect-free product

A good injection molded product is not created at the machine alone, but through collaboration between designer, material supplier and injection molder. The earlier these parties look at the product together, the smaller the chance of defects in production.

At Fleur Plastics, we look at design, material and mold from the very start, so that problems are prevented rather than fixed afterwards. Are you running into one of these defects, or do you want to stay ahead of them with a new product? Contact us and we will work out the best approach together.

Our customers
  • File (14).jpg
  • File (13).jpg
  • File (12).jpg
  • File (11).jpg
  • File (10).jpg
  • File (9).jpg
  • File (8).jpg
  • File (7).jpg
  • File (6).jpg
  • File (5).jpg
  • File (4).jpg
  • File (3).jpg
  • File (2).jpg
  • File (1).jpg
  • File.jpg
Our solutions ›
Receive our newsletter!

Subscribe to our newsletter to receive our latest news